Welding & project operations
Welding Electrode Number Meaning: E7018, E6013 Decoder
Type a welding electrode or wire classification, such as E6013, E7018-1 H4R, ER70S-6, E71T-1C, E308L-16 or ER5356, and this decoder explains every part: the minimum tensile strength, the welding positions, the covering type and current, alloy and toughness suffixes, hydrogen level, shielding gas and what the filler is meant for.
- Free, no sign-up
- Runs in your browser
- Built for Islamabad & Rawalpindi
This free calculator runs in your browser and needs JavaScript. If it does not load, call or WhatsApp us on +92 304 2435577 and we will do the calculation for you.
Electrode boxes in Pakistani markets carry AWS classifications, sometimes alongside brand names that say nothing about the rod. Reading the classification tells you whether an E6013 or an E7018 is the right rod for the job, and what storage and current it needs.
What This Tool Does
It reads AWS A5.1 and A5.5 stick electrodes, A5.18 solid wires, A5.20 flux-cored wires, A5.4 and A5.9 stainless fillers and A5.10 aluminium fillers, and flags points such as low-hydrogen storage and aluminium alloy compatibility.
Who It Is For
- Welders buying rods and wire.
- Supervisors and storekeepers checking deliveries.
- Trainees learning classifications.
How To Use It
- Type the classification from the box or packet, or tap one of the examples.
- Press Decode.
- Read the meaning of each part and any warnings.
How The Calculation Works
In AWS stick electrodes E XX Y Z: E is electrode, XX the minimum tensile strength in ksi (70 = 70,000 psi ≈ 480 MPa), Y the positions (1 all positions, 2 flat and horizontal fillets, 4 includes vertical-down) and the last two digits together the covering and current type (13 rutile, 18 low-hydrogen iron powder). Suffixes add alloy (A1, B2, C1), toughness (-1), diffusible hydrogen (H4, H8, H16) and moisture resistance (R).
Worked Example
E7018-1 H4R.
| Input or result | Value |
|---|---|
| 70 | 70 ksi (≈ 483 MPa) minimum tensile strength |
| 1 | all positions |
| 18 | low-hydrogen potassium covering with iron powder, AC or DCEP |
| -1 | improved impact toughness |
| H4 | at most 4 mL diffusible hydrogen per 100 g |
| R | moisture-resistant covering |
A rod for structural steel that must be stored dry, unlike E6013, which is a general-purpose rutile rod.
Features And Benefits
- Covers stick, MIG, flux-cored, stainless and aluminium fillers.
- Warnings for storage and compatibility.
- Plain-language meaning of each part.
Assumptions And Accuracy Limits
- ISO 2560 and ISO 14341 names use a different system and are not decoded.
- It explains a classification; it does not approve a filler for a job.
Common Mistakes To Avoid
- Storing E7018 in the open. Low-hydrogen rods pick up moisture and lose their benefit; keep them in a rod oven or sealed tin.
- Reading the brand, not the classification. Two boxes with different brand names can contain the same rod type.
- Using 308L on mild steel to stainless joints. Use 309L for dissimilar joints.
Buying Electrodes In Islamabad And Rawalpindi
Electrodes sold in local markets carry the AWS classification on the box, often alongside a brand name. E6013 is the common general-purpose rod; E7018 is used where strength and crack resistance matter. Check the packet date and keep low-hydrogen rods dry, especially in the monsoon.
Frequently Asked Questions
What does E7018 mean?
E electrode, 70 ksi minimum tensile strength, 1 all positions, 8 (with the 1) low-hydrogen potassium covering with iron powder for AC or DCEP.
What is the difference between E6013 and E7018?
E6013 is a rutile, easy-to-use rod with 60 ksi strength for general work. E7018 is a low-hydrogen rod with 70 ksi strength for structural and crack-sensitive work, and must be kept dry.
What does ER70S-6 mean?
A solid wire or rod for gas-shielded welding, 70 ksi, with the highest manganese and silicon of the series, so it tolerates some mill scale.
Which filler for 304 stainless?
Usually 308L. Use 309L to join stainless to mild steel.
ER4043 or ER5356 for aluminium?
4043 flows well and cracks less on 6xxx alloys and castings; 5356 is stronger and matches colour after anodising. Check the base alloy.
Related Free Tools
- Welding Process Selection AssistantCompare stick, MIG, flux-cored and TIG for your metal, thickness, site and skill level.
- Weld Volume, Filler & Consumables EstimatorEstimate deposited weld metal and electrode purchase from weld size, length and efficiency.
- Carbon Equivalent (CE, Pcm, CET) CalculatorCalculate CE (IIW), Pcm and CET from a steel's chemical composition, each formula shown separately.
- Shielding Gas Cylinder Runtime & Cost PlannerFind how long an argon, CO2 or mixed-gas cylinder lasts at your flow rate and what the gas costs per job.
Get A Measured Quotation
Ramzan Steel Works uses the right consumable for each job in its welding work across Islamabad and Rawalpindi.