Welding & project operations
Welding Defects, Causes And Remedies Guide
This guide covers the common welding defects: porosity, undercut, lack of fusion, lack of penetration, spatter, cracking, slag inclusions, distortion, uneven bead and burn-through. For each it describes what the defect looks like, the likely causes, what to check, possible corrections and when a professional should be involved. Add the defects you found to a report with your notes and print it.
- Free, no sign-up
- Runs in your browser
- Built for Islamabad & Rawalpindi
This free calculator runs in your browser and needs JavaScript. If it does not load, call or WhatsApp us on +92 304 2435577 and we will do the calculation for you.
Most weld defects come from a small set of causes: dirty metal, damp consumables, wrong current or speed, and poor fit-up. Working through the checks in order usually finds the cause faster than changing settings at random.
What This Tool Does
It shows structured guidance for each defect and builds a printable troubleshooting report from the defects you add.
Who It Is For
- Welders fixing a recurring problem.
- Supervisors training new welders.
- Clients understanding an inspection finding.
How To Use It
- Choose the defect you see.
- Work through the checks.
- Add it to the report and write your notes.
- Print the report.
How The Calculation Works
The guidance is general welding practice, organised by defect. It is not specific to any code; acceptance limits come from the job specification.
Worked Example
Porosity on MIG welds made outdoors.
| Input or result | Value |
|---|---|
| Likely cause | shielding gas blown away by wind |
| Check | flow at the torch and drafts |
| Correction | shelter the arc, or switch to self-shielded wire or stick |
Grind out the porous metal before re-welding.
Features And Benefits
- Ten defects covered.
- Causes, checks and fixes in order.
- Printable report.
Assumptions And Accuracy Limits
- Visual appearance cannot confirm internal quality.
- Acceptance limits come from the job specification or code.
Common Mistakes To Avoid
- Turning up the current for every problem. Many defects come from too much current, not too little.
- Welding over a crack. It must be ground out completely first.
- Ignoring damp rods. Porosity and cracking often start with moisture.
Weld Repairs In Islamabad And Rawalpindi
Humid monsoon months raise porosity and hydrogen cracking risk from damp consumables, and wind affects site MIG work. Ramzan Steel Works repairs cracked gates, frames and brackets across Islamabad and Rawalpindi, and grinds out defects before re-welding.
Frequently Asked Questions
What causes porosity in welding?
Gas trapped in the weld, usually from moisture, rust, oil, paint or zinc, or from poor gas shielding.
What causes undercut?
Too much current, too fast travel, a long arc or the wrong electrode angle.
Can cracks in welds be repaired?
Usually, by grinding out the whole crack and re-welding, but the cause must be found first, and for load-bearing welds a qualified person should decide.
How do I reduce welding distortion?
Weld only the size needed, balance welds, tack and clamp, use backstep or intermittent welds, and pre-set the parts.
Related Free Tools
- Welding Visual Inspection Report GeneratorRecord welds, observations, defects, results and photos, then print a clean visual inspection report.
- Welding Process Selection AssistantCompare stick, MIG, flux-cored and TIG for your metal, thickness, site and skill level.
- Welding Symbols Chart, Decoder & PracticeBuild a welding symbol, see what it means in plain words, and test yourself with practice questions.
- Welding Joint Preparation & Bevel Geometry CalculatorDraw a V, X, bevel or square butt preparation to scale and get groove area and weld metal per metre.
Get A Measured Quotation
If a weld needs repair rather than troubleshooting, Ramzan Steel Works carries out welding repairs across Islamabad and Rawalpindi.